| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 103 - 138 MPa | 14900 - 20000 psi | |
|
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **)
Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically..
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | Injection Molding |
|
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade
Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus..
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
|
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Injection Pressure | 69.0 - 138 MPa | 10000 - 20000 psi | |
|
Lavergne VYPET VNT 1020 Polyester-PC Alloy
The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
|
|||
| Injection Pressure | 69.0 - 138 MPa | 10000 - 20000 psi | |
|
Lavergne VYPET VNT 1021 Polyester-PC Alloy
The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
|
|||
| Injection Pressure | 69.0 - 138 MPa | 10000 - 20000 psi | |
|
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate
Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl..
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
|
MRC Polymers NAXELLâ„¢ PC110-919 General Purpose Polycarbonate, Medium High MFR
Polycarbonate for colorable productsMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedCan be clear to color matchedNot for products that req..
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | |
|
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66
Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman.
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | Initial |
|
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated
Data provided by Clariant Masterbatches
|
|||
| Injection Pressure | 34.5 - 138 MPa | 5000 - 20000 psi | |
|
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
|
|||
| Injection Pressure | 8.27 - 138 MPa | 1200 - 20000 psi | Average value: 34.8 MPa Grade Count:4 |
|
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
|
|||
| Injection Pressure | 68.9 - 138 MPa | 10000 - 20000 psi | Average value: 101 MPa Grade Count:5 |
|
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..
|
|||