Polymer Property : Injection Pressure = 30.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Injection Pressure 30.0 - 124 MPa
4350 - 18000 psi
Average value: 93.1 MPa Grade Count:13
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Injection Pressure 30.0 - 100 MPa
<br>@Time 2.00 - 10.0 sec
4350 - 14500 psi
<br>@Time 0.000556 - 0.00278 hour
Gromax 1140LH TPE
Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject..
Injection Pressure 30.0 - 100 MPa
<br>@Time 2.00 - 10.0 sec
4350 - 14500 psi
<br>@Time 0.000556 - 0.00278 hour
Gromax 1155LL TPE
1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex..
Injection Pressure 30.0 - 100 MPa
<br>@Time 2.00 - 10.0 sec
4350 - 14500 psi
<br>@Time 0.000556 - 0.00278 hour
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner JEPP2056 PP For Automotive Parts
Applications: BumpersInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 80.0 MPa
4350 - 11600 psi
Zhejiang Juner JEPPB003 High Glossy PP
Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 70.0 MPa
4350 - 10200 psi
Zhejiang Juner JEPPB006 High Glossy PP
Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 40.0 MPa
4350 - 5800 psi
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP201-G30 PP For Automotive Parts
Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP6-1JE PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 90.0 MPa
4350 - 13100 psi
Zhejiang Juner PP8 PP For Automotive Parts
Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd.
Injection Pressure 30.0 - 40.0 MPa
4350 - 5800 psi
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 45.0 MPa
4350 - 6530 psi
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Toyobo GLAMIDE® TY-145TZ Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 70.0 MPa
4350 - 10200 psi
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 40.0 MPa
4350 - 5800 psi
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 70.0 MPa
4350 - 10200 psi
Toyobo GLAMIDE® TY-791GT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Injection Pressure 30.0 - 60.0 MPa
4350 - 8700 psi
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Injection Pressure 30.0 MPa
4350 psi
Recommended Molding Pressure.
Asahi Glass Fluon® G307 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
Injection Pressure 30.0 MPa
4350 psi
Recommended Molding Pressure.
Asahi Glass Fluon® G340 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
Injection Pressure 30.0 - 55.0 MPa
4350 - 7980 psi
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Injection Pressure 30.0 - 124 MPa
4350 - 18000 psi
Average value: 87.0 MPa Grade Count:5
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Injection Pressure 30.0 MPa
4350 psi
Recommended Molding Pressure.
Asahi Glass Fluon® G350 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.