Processing Properties Metric English Comments
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Polykemi AB POLYfill PP CIP16020FCS Polypropylene, Fast Cycle
Information provided by Polykemi AB
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Polykemi AB POLYfill PP CQX10030E10 Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH GF8030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPHC GF3030 PD2 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC GF15030 PD2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized
Information provided by Polykemi AB
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE.
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE.
Injection Pressure 40.0 - 100 MPa
5800 - 14500 psi
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Injection Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Injection Molding (Injection pressure should be increased when molding thin wall parts. Pressure up to 75 bar can be used here.)
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE.
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPH GF10020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Polykemi AB POLYfill PPHC EP1001F Polypropylene
Information provided by Polykemi AB