Polymer Property : Injection Pressure = 6.89 MPa Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® OBC 4755A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL 83-F943D22-NT Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL EF-6100 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL EF-6109 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1025-85 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1425A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-2575F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-2635A Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer
Uses: Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-4002 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-6085 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Uniprene® UN-2420D Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TELC 1025-70 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
CPT C-Flex® R70-116 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..