| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler
Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o.
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom PLASTAMID® 6 BT N 32 B PA6
Basic type PA 6 for compounding, for general use. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o.
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom PLASTAMID® 6 BT PA6
Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Informa..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom PLASTAMID® 6 GF 15 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 15% glass fiber. Application: applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom PLASTAMID® 66 GF 30 TS 002 PA66 reinforced with glass fiber, heat stabilized
PA66 for injection molding, reinforced with 30 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying pa..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc
FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler
Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling
FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 66 GF 20 FRO 4 PP, 20% glass fibre, flame retardant
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, with decreased flammability. Used in the electrical industry - teroderately increased toughness an..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 6 G 5 Polyamide 6, 5% Graphite
FeaturesPA 6 for injection moulding with addition of 5% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, slid..
|
|||
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 6 GF 15 T 25 Polyamide 6, 15% Glass Fiber, 25% Micronized Talc
FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form / no screw after co..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 10 PA66, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength
FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc
FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre
FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber
FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant
FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID 66 HI Polyamide 66, Impact Grade
FeaturesModified with thermoplastic reactive elastomer, determined for mouldings with high toughness also at low temperatures. Eligible application for ski-shoes, helmets for sport and other safety..
|
|||
| Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi | |
|
Plastcom SLOVAMID® 6/66 GF 15 GB 15 PA6/66 reinforced with glass fiber, glass beads
PA 6 and PA 66 alloy for injection molding, reinforced with 15% glass fiber and 15 % glass beads, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders ..
|
|||
| Injection Pressure | 70.0 - 100 MPa | 10200 - 14500 psi | |
|
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||