Processing Properties Metric English Comments
Pot Life 120 min
120 min
NextGen Adhesives P907-10 Optical Assembly Adhesive
Description: NGAC P907-10 is a low viscosity and optically clear adhesive system that is specifically formulated for bonding and potting applications involving optical components and assemblies.Adva..
Pot Life 120 min
120 min
Resin Technology Group DPE110698-1 Two component Potting Compound
Resin Technology Group DPE110698-1 Two component Potting CompoundClear, fire retardant, low viscosity potting compound.
Pot Life 120 - 240 min
120 - 240 min
Abatron KromaKote 8901-8 Polyurethane Coating  (discontinued **)
2-component system for outstanding performance in normal, industrial, marine and corrosive environments. Superb combination of chemical, solvent, abrasion and weather resistance.Suggested Uses: Pro..
Pot Life 120 - 180 min

@Temperature 20.0 °C
120 - 180 min

@Temperature 68.0 °F
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Pot Life 120 - 120 min

@Temperature 80.0 - 80.0 °C
120 - 120 min

@Temperature 176 - 176 °F
Average value: 120 min Grade Count:1
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
4 fl. Oz.; ASTM D2471
Fibre Glast 2000 / 2120 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Pot Life 120 min
120 min
Lord Adhesives 3170 Two-component, high cold strength, cryogenic application Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 120 - 180 min
120 - 180 min
Ready for topcoating
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free
Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul..
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
Momentive Performance Materials RTV8112 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Pot Life 120 - 150 min
120 - 150 min
100 gram mass
Master Bond EP21SC-1 Two Component Epoxy Resin System
Product Description: Master Bond Polymer System EP21SC-1 is a two component epoxy system featuring abrasion resistance. This high performance compound utilizes silicon carbide as a filler material a..
Pot Life 120 min
120 min
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive
TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, an..
Pot Life 120 min
120 min
25 grams
Tra-Con Tra-Bond F123MV Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F123 MV is a fast cure, medium viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminati..
Pot Life 120 min
120 min
2X initial viscosity
Tra-Con Tra-Bond F253M Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F253M is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mix..
Pot Life 120 min
120 min
Tra-Con Tra-Bond FS302 Easy-Flow No-Sag Epoxy Adhesive
TRA-BOND FS-302 is a thixotropic room temperature cure epoxy adhesive system developed for structural bonding applications on vertical or overhead surfaces where its no-sag characteristics are criti..
Pot Life 120 min
120 min
Tra-Con Tra-Cast F311 Optically Transparent Semi-Flexible Casting System
TRA-CAST F311 is a clear, low viscosity epoxy formulation developed for molding, embedding, casting and potting applications where clarity, toughness, long pot-life and superior impact properties ar..
Pot Life 120 min
120 min
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive
TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a ..
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
100 grams
Trelleborg Emerson & Cuming Eccobond® 15 Clear Variable Hardness Catalyst
Emerson & Cuming 15 Clear Eccobond® Variable Hardness CatalystEasy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields ..
Pot Life 120 - 360 min

@Temperature 25.0 °C
120 - 360 min

@Temperature 77.0 °F
100 grams
Cytec (Conap) FR-1274 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 120 min
120 min
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra..
Pot Life 120 min
120 min
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste
Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de..
Pot Life 120 min
120 min
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive
EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional ..
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
200 g
Abatron AboCast/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Pot Life 120 min
120 min
Abatron 8509-3 A/B Carbon-Filled Electrically Conductive Epoxy Compound
8509-3 A/B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements.
Pot Life 120 min
120 min
100 g
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Pot Life 120 - 180 min
120 - 180 min
Abatron AboCast 50-11/AboCure 50-4 Epoxy
AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A..
Pot Life 120 - 150 min
120 - 150 min
Mass: 100g; TM R050-19
Resinlab® EP1200LV Casting Resin
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an..