| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life | 10 - 20 min | 10 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® UR3001HP Black Urethane Encapsulant
Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e..
|
|||
| Pot Life | 10 - 20 min | 10 - 20 min | Time before parts must be mated |
|
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | |
|
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | 100 gm mass |
|
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy
Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | 100 gram batch |
|
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or ..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | 100 gram mass |
|
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room ..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | |
|
Loctite® 3951 Gap filling, flexible Urethane Adhesive
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap..
|
|||
| Pot Life |
15
-
20
min @Temperature 24.0 °C |
15
-
20
min @Temperature 75.2 °F |
4 oz. mass |
|
BCC Products BC 6004 Epoxy Surface Coat
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi..
|
|||
| Pot Life |
16
-
20
min @Temperature 24.0 °C |
16
-
20
min @Temperature 75.2 °F |
|
|
BCC Products BC 8160 Urethane Casting
BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly..
|
|||
| Pot Life |
16
-
20
min @Temperature 24.0 °C |
16
-
20
min @Temperature 75.2 °F |
work life |
|
BCC Products BC 8860 Polyurethane Elastomer
BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig..
|
|||
| Pot Life |
18
-
20
min @Temperature 24.0 °C |
18
-
20
min @Temperature 75.2 °F |
|
|
BCC Products BC 8870 Polyurethane Elastomer
BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting ..
|
|||
| Pot Life | 15 - 20 min | 15 - 20 min | Mass: 50g; TM R050-19 |
|
Resinlab® UR3001HP Clear Urethane Encapsulant
Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e..
|
|||
| Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
|
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
|
|||
| Pot Life | 10 - 20 min | 10 - 20 min | Mass: 100g |
|
Resinlab® UR3005 Two Part Urethane Elastomer
Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen..
|
|||