Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 300 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Pot Life 300 min
300 min
Parker Chomerics CHO-SHIELD® 4966 Conductive Silicone Coating
Conductive Silicone Coating. This is a conductive silver-filled silicone coating. This three-component system is capable of providing 60 dB of shielding effectiveness above 30 MHz. The coating utili..
Pot Life 300 min

@Temperature 23.0 °C
300 min

@Temperature 73.4 °F
2X Starting Viscosity
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Pot Life >= 300 min
>= 300 min
Resin Technology Group DPE080697-1 Two component Potting Compound
Resin Technology Group DPE080697-1 Two component Potting CompoundClear, 2 part, UV/Heat/Room temperature cure epoxy potting compound.
Pot Life >= 300 min
>= 300 min
Resin Technology Group DPE080697-1 Two component Potting Compound
Resin Technology Group DPE080697-1 Two component Potting CompoundClear, 2 part, UV/Heat/Room temperature cure epoxy potting compound.
Pot Life >= 300 min
>= 300 min
Abatron 2230 A/B Filled Potting Compound  (discontinued **)
Universal casting, potting, and encapsulating for magnets and electric black and colors. 4/1 variable ratio.Information provided by Abatron.
Pot Life 300 min

@Temperature 23.0 °C
300 min

@Temperature 73.4 °F
2X Starting Viscosity
Parker Chomerics THERM-A-FORM T646 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Pot Life 300 min
300 min
Henkel Hysol EA 9380.05 Paste Adhesive System
High degree of cure after a low temperature cure time that offers strength, toughness and high temperature resistance of heat curing film adhesives with greater flexibility and ease of use. Can be a..
Pot Life 300 min
300 min
Tra-Con Tra-Bond F211 General Purpose Fiber Optic Epoxy Adhesive
TRA-BOND F211 is a general purpose fiber optic epoxy adhesive recommended for bonding and small volume potting applications where superior wetting and physical properties are needed at both high and..
Pot Life 300 min
300 min
Tra-Con Tra-Bond FS443 Color Keyed Thixotropic Epoxy Adhesive
TRA-BOND FS443 is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating s..
Pot Life 300 min
300 min
25 grams
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunicatio..
Pot Life 300 min
300 min
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive
TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r..
Pot Life 300 min
300 min
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive
Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. ..
Pot Life 300 - 360 min
300 - 360 min
Abatron AboCast 8502-5/AboCure 8502-5 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-5/AboCure 8502-5 is a rigid, colorless, low-exotherm epoxy casting compound for spherical masses up to 500 grams. It is a 2-component structural and dielectric liquid system with extrem..
Pot Life 300 - 480 min

@Temperature 25.0 °C
300 - 480 min

@Temperature 77.0 °F
1-2 lbs
Abatron AboCast/AboCure 4-4/50-17 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLongest pot lifeLarges..
Pot Life 300 - 480 min
300 - 480 min
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste
BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical..
Pot Life 300 - 480 min
300 - 480 min
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid
Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin..
Pot Life 300 - 480 min
300 - 480 min
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste
Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris..
Pot Life 300 - 480 min
300 - 480 min
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste
Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha..
Pot Life 300 min
300 min
100 g
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Pot Life 300 - 480 min
300 - 480 min
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid
Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin..
Pot Life 300 - 480 min
300 - 480 min
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste
SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra..
Pot Life >= 300 min
>= 300 min
Epoxyset Epoxibond EB-177 Unfilled Epoxy Adhesive
A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc...
Copyright © lookpolymers.com All Rights Reserved