| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
|
|||
| Pot Life |
4.0
min @Temperature 21.1 °C |
4.0
min @Temperature 70.0 °F |
Working Time |
|
Protective Coating PC-Clear™ Clear Liquid Epoxy
PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include..
|
|||
| Pot Life |
4.0
min @Temperature 25.0 °C |
4.0
min @Temperature 77.0 °F |
|
|
Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV
Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the..
|
|||
| Pot Life |
4.0
min @Temperature 25.0 °C |
4.0
min @Temperature 77.0 °F |
|
|
Parker Chomerics Tecknit CON/RTV-Ni 2 Part Nickel Filled RTV
Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | Time before parts must be mated |
|
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
|
|||
| Pot Life | 4.0 - 5.0 min | 4.0 - 5.0 min | Time before parts must be mated |
|
Lord Adhesives 7542B Two-Component Urethane Adhesive
Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe..
|
|||
| Pot Life |
4.0
-
5.0
min @Temperature 25.0 °C |
4.0
-
5.0
min @Temperature 77.0 °F |
|
|
Lord Adhesives Thermosetâ„¢ UR-322 Two Component Urethane Potting Compound
Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA821 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
|
|||
| Pot Life |
4.0
-
4.5
min @Temperature 24.0 °C |
4.0
-
4.5
min @Temperature 75.2 °F |
50 gram mass |
|
BCC Products BC 5200 Kwik-Set Adhesive
BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil..
|
|||