| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life |
40320
min @Temperature 25.0 °C |
40320
min @Temperature 77.0 °F |
|
|
Lord Adhesives Circalokâ„¢ EP-729 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ EP-729 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by..
|
|||
| Pot Life |
40320
min @Temperature 25.0 °C |
40320
min @Temperature 77.0 °F |
|
|
Lord Adhesives Circalokâ„¢ EP-937 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by..
|
|||
| Pot Life |
40320
min @Temperature 25.0 °C |
40320
min @Temperature 77.0 °F |
|
|
Lord Adhesives Circalokâ„¢ EP-939 Epoxy Board Level Encapsulant
LORD Thermosetâ„¢ EP-939 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® B9021 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
|
|||
| Pot Life | 40320 min | 40320 min | Closed container |
|
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® E3035T-2 Electrically Conductive Epoxy
Product Description: EPO-TEK® E3035T-2 is a single component, silver-filled epoxy for semiconductor die attach, as well as SMD attach on hybrid circuits.Advantages & Application Notes: This epoxy c..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® E3037 Epoxy
Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® ED1020 Epoxy
Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Its unique features include exce..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® EM127 Electrically Conductive Epoxy
Product Description: EPO-TEK® EM127 is a single component, heat curable, electrically conductive epoxy adhesive for semiconductor IC and LED die attach applications.Advantages & Application Notes: ..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35-175MP is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-elec..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H35-175MPT Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35MPT is a single component, silver-filled, electrically conductive epoxy designed for military hybrid die and component attach. High viscosity version of EPO-TEK® H..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H37-MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H37-MP is a single component, electrically conductive, thixotropic silver-filled adhesive for die-attach and SMD attach inside hybrid microelectronic packages. Also av..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® E3035 Electrically Conductive Adhesive
Product Description: EPO-TEK® E3035 is a single component, silver-filled epoxy for hybrid die and component attach.Advantages & Application Notes: Performs exceptionally well as a die attach for sm..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H31 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31 is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-electronic..
|
|||
| Pot Life | 40320 min | 40320 min | |
|
Epoxy Technology EPO-TEK® H37-MPT Epoxy
Material Description: A single component, silver-filled and electrically conductive adhesive designed for semiconductor die attach and bonding SMDs for hybrid microelectronic packaging. It is certi..
|
|||