| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life |
40.0
-
50.0
min @Temperature 50.0 - 50.0 °C |
40.0
-
50.0
min @Temperature 122 - 122 °F |
Average value: 45.0 min Grade Count:1 |
|
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
|
|||
| Pot Life |
45.0
-
50.0
min @Temperature 25.0 °C |
45.0
-
50.0
min @Temperature 77.0 °F |
1 lbm |
|
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Pot Life |
45.0
-
50.0
min @Temperature 25.0 °C |
45.0
-
50.0
min @Temperature 77.0 °F |
1 lbm |
|
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Pot Life |
40.0
-
50.0
min @Temperature 50.0 °C |
40.0
-
50.0
min @Temperature 122 °F |
1 lbm |
|
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||