| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | Mass: 50g; TM R050-19 |
|
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | Time before parts must be mated |
|
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA821 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..
|
|||
| Pot Life | 4.0 - 6.0 min | 4.0 - 6.0 min | |
|
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
|
|||
| Pot Life |
5.0
-
6.0
min @Temperature 25.0 °C |
5.0
-
6.0
min @Temperature 77.0 °F |
1 lb. mass |
|
BCC Products Kwik Kast BC 8645 Urethane Casting
BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing..
|
|||
| Pot Life |
5.0
-
6.0
min @Temperature 24.0 °C |
5.0
-
6.0
min @Temperature 75.2 °F |
1 lb. mass |
|
BCC Products Kwik Kast BC 8650 Urethane Casting
BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl..
|
|||
| Pot Life |
5.0
-
6.0
min @Temperature 24.0 °C |
5.0
-
6.0
min @Temperature 75.2 °F |
1 lb. mass |
|
BCC Products LIK-WOOD BC 8007 Urethane Casting
Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an..
|
|||