Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 60.0 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Pot Life 60.0 min
<br>@Temperature 23.0 °C
60.0 min
<br>@Temperature 73.4 °F
2X Starting Viscosity
Parker Chomerics THERM-A-FORM 1642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Pot Life 60.0 min
<br>@Temperature 23.0 °C
60.0 min
<br>@Temperature 73.4 °F
2X Starting Viscosity
Parker Chomerics THERM-A-FORM T642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Pot Life 60.0 - 90.0 min
60.0 - 90.0 min
Northstar Polymers MYP-V40A Polyurethane Filler Gel
This polyurethane casting material is developed for applications that require inexpensive liquid resin filler such as encapsulation of a large electric components or puncture-free tire for low-speed..
Pot Life 60.0 - 120 min
<br>@Temperature 20.0 °C
60.0 - 120 min
<br>@Temperature 68.0 °F
Permabond ET505 Epoxy Resin
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
Pot Life 60.0 min
<br>@Temperature 23.9 °C
60.0 min
<br>@Temperature 75.0 °F
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown &nbsp;(discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren..
Pot Life 60.0 - 1440 min
60.0 - 1440 min
Average value: 630 min Grade Count:5
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
4 fl. Oz.; ASTM D2471
Fibre Glast 2000 / 2060 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Pot Life 60.0 min
<br>@Temperature 23.9 °C
60.0 min
<br>@Temperature 75.0 °F
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon
Pot Life 60.0 min
<br>@Temperature 23.9 °C
60.0 min
<br>@Temperature 75.0 °F
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey
Information provided by ITW Devcon
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
Momentive Performance Materials RTV21 Pink General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
Momentive Performance Materials RTV6156 Clear Potting/Encapsulating Gel
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
2X initial viscosity
Tra-Con Tra-Bond 216C05
Information provided by Tra-Con Inc.
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
100 grams
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst
Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applicati..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
100 grams
Cytec (Conap) RN-1200 / EA-87 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
100 grams
Cytec (Conap) RN-1210 / EA-87 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
Pot Life 60.0 - 80.0 min
<br>@Temperature 25.0 °C
60.0 - 80.0 min
<br>@Temperature 77.0 °F
1 lbm
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Pot Life <= 60.0 min
<br>@Temperature 25.0 °C
<= 60.0 min
<br>@Temperature 77.0 °F
100 g
Armstrong A-2/W Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
100 gm mass
Aremco Aremco-Bond™ 2220 High Performance Epoxide
Ceramic-Filled, High Chemical Resistance, Machinable. For Repairing Deeply-Corroded Parts.
Pot Life 60.0 min
60.0 min
100 grams, uncured
Atom Adhesives AA-BOND 2110 Epoxy Adhesive
AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no..
Pot Life 60.0 - 120 min
60.0 - 120 min
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina
Fine grain castable for potting and producing small tools.
Pot Life 60.0 - 120 min
60.0 - 120 min
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide
Single-part castable ceramic exhibiting high strength and thermal conductivity.
Pot Life 60.0 min
60.0 min
uncured
Atom Adhesives AA-BOND 428 Epoxy Adhesive
AA-BOND 428 is a two part, heat-resistant and low exotherm, epoxy adhesive formulation. It is a 100% solid epoxy adhesive, with superior chemical resistance and shear strength. AA-BOND 428 contains ..
Pot Life 60.0 min
60.0 min
uncured
Atom Adhesives AA-BOND F253 Epoxy Adhesive
AA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status.Appearance: Unmixed-Light Yellow; Mixed – Greenish..
Pot Life 60.0 min
60.0 min
uncured
Atom Adhesives AA-DUCT 903 Epoxy Adhesive
AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha..
Pot Life 60.0 min
60.0 min
uncured
Atom Adhesives AA-BOND 2170 Epoxy Adhesive
AA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrate. A..
Pot Life 60.0 min
60.0 min
uncured
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive
AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir..
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
100 gm mass
Aremco Aremco-Bond™ 2320 High Performance Epoxide
Toughened, Unfilled, Fast-Setting, BPA Free, 2:1, High Peel & Shear Strength
Pot Life 60.0 min
<br>@Temperature 25.0 °C
60.0 min
<br>@Temperature 77.0 °F
4 fl. Oz.; ASTM D2471
Fibre Glast RAE 2426 / 2177 Epoxy &nbsp;(discontinued **)
Information provided by Fibre Glast Developments Corporation.
Copyright © lookpolymers.com All Rights Reserved