Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Pot Life 60 - 75 min
60 - 75 min
100 grams
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy
Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera..
Pot Life 60 - 75 min
60 - 75 min
200 gram mass
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive
Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or ..
Pot Life 60 - 75 min
60 - 75 min
200 gram mass
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Pot Life 60 - 75 min
60 - 75 min
100 gram mass
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy
Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl..
Pot Life 45 - 75 min
45 - 75 min
100 gram batch
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements
Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit..
Pot Life 60 - 75 min
60 - 75 min
100 gm mass
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive
Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit..
Pot Life 60 - 75 min
60 - 75 min
100 gram mass
Master Bond EP21CLV Two Component Epoxy System
Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a..
Pot Life 60 - 75 min
60 - 75 min
100 gram batch
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
Pot Life 45 - 75 min
45 - 75 min
100 gram mass
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System
Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi..
Pot Life 45 - 75 min
45 - 75 min
100 gram batch
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o..
Pot Life 45 - 75 min
45 - 75 min
100 gram batch
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an..
Pot Life 60 - 75 min
60 - 75 min
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy
Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and c..
Pot Life 45 - 75 min
45 - 75 min
100 gram mass
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
Pot Life 45 - 75 min
45 - 75 min
100 gram batch
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy
Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding ..