Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 90 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Pot Life 90 - 120 min
90 - 120 min
Mass: 100g; TM R050-19
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Pot Life 90 min
90 min
Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life 90 min
90 min
Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life >= 90 min
>= 90 min
Abatron 225 A/B Filled Potting Compound  (discontinued **)
Dielectric structural potting and embedding adhesive. Higher impact, green and most colors. 10/3 variable ratio.Information provided by Abatron.
Pot Life >= 90 min
>= 90 min
catalyzed with Stretch Effect B
ACC Stretch Effect QSI Quantum Silicones Stretch Effect 22 Durometer Addition Cure Translucent Moldmaking Material &amp
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, fast demold time, high elongation, excellent flexibility. Applications: special effects, skin replicat..
Pot Life 90 - 150 min
90 - 150 min
Time before parts must be mated
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 90 - 120 min
<br>@Temperature 25.0 °C
90 - 120 min
<br>@Temperature 77.0 °F
54g mass
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..
Pot Life 90 - 105 min
90 - 105 min
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Pot Life 90 - 120 min
90 - 120 min
Curing
Silikony Polskie Gumosil M Silicone Rubber
Flexible with good tearing resistance
Pot Life >= 90 min
>= 90 min
100 gram mass
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation ..
Pot Life 90 - 120 min
90 - 120 min
100 gram mass
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System
Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t..
Pot Life 90 - 120 min
90 - 120 min
100 gram mass
Master Bond EP21NDFG Two component epoxy compound for high performance applications
Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency..
Pot Life >= 90 min
>= 90 min
100 gram mass
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra..
Pot Life 90 - 120 min
90 - 120 min
100 gram mass
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy
Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one ..
Pot Life 90 - 120 min
90 - 120 min
100 gram mass
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating
Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving..
Pot Life 90 - 150 min
90 - 150 min
100 grams
Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System
Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati..
Pot Life 90 min
90 min
100 grams
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System
TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit..
Pot Life 90 min
90 min
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy
Material Description: A two component, optically clear, flexible epoxy adhesive designed for optical applications within semiconductor, fiber optic and medical industries. An alternative to EPO-TEK..
Pot Life 90 min
90 min
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
Pot Life 90 min
90 min
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive
Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p..
Pot Life 90 min
90 min
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy
Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing..
Pot Life 90 min
90 min
Epoxy Technology EPO-TEK® T7109-18 Electrically Insulating Epoxy Paste
Material Description: A flexible, electrically insulating epoxy paste designed for low stress and heat dissipation applications. Alternative to EPO-TEK® T7109-17.Information Provided by Epoxy Tec..
Pot Life 90 min
<br>@Temperature 25.0 °C
90 min
<br>@Temperature 77.0 °F
500 g
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy
AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thi..
Pot Life 90 min
90 min
BASF Master Builders Solutions ChemRex® CX Concrete Floor Primer - Epoxy
CX Concrete Floor Primer is a waterborne epoxy primer for concrete substrates. It is designed to manage and reduce moisture vapor emission (out-gassing) of concrete slabs by controlling the rate of..
Pot Life 90 min
<br>@Temperature 24.0 °C
90 min
<br>@Temperature 75.2 °F
2 lb. mass
BCC Products BC 7009-1 Epoxy Casting
BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces..
Pot Life 90 min
90 min
10 grams
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive
TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a..
Pot Life 90 min
90 min
Loctite® Durabond® E-90FL Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Pot Life 90 - 120 min
90 - 120 min
Mass: 100g; TM R050-19
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat..
Copyright © lookpolymers.com All Rights Reserved