Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 100 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7662/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 100 - 110 °C

@Time 7200 - 10800 sec
212 - 230 °F

@Time 2.00 - 3.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 100-7126 VP Thermoplastic polyurethane, with PTFE
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Drying Temperature 100 - 110 °C

@Time 7200 - 10800 sec
212 - 230 °F

@Time 2.00 - 3.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Drying Temperature 100 °C

@Time 14400 sec
212 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Horizontal Oven
Zhejiang Juner PC Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Horizontal Oven
Zhejiang Juner PC/ABS Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Chute Hot-Wind
Zhejiang Juner PC/PBT Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 28800 sec
212 °F

@Time 8.00 hour
Horizontal Oven
Zhejiang Juner PC/PBT Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 °C

@Time 18000 sec
212 °F

@Time 5.00 hour
Horizontal Oven
Zhejiang Juner PC-3-1 Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 100 °C

@Time 14400 sec
212 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC/ABSz-4 Alloy
Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 100 - 140 °C

@Time 7200 - 14400 sec
212 - 284 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..