Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 120 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Drying Temperature 120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-7753/BL PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
Drying Temperature 120 °C

@Time 7200 - 18000 sec
248 °F

@Time 2.00 - 5.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Drying Temperature 120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® 80-8470 Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105/BL8052 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
Lehmann & Voss LUVOCOM® 1105-7596/BL PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
Drying Temperature 120 °C

@Time 7200 - 18000 sec
248 °F

@Time 2.00 - 5.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 120 °C

@Time 7200 - 18000 sec
248 °F

@Time 2.00 - 5.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Drying Temperature 120 °C

@Time 7200 - 14400 sec
248 °F

@Time 2.00 - 4.00 hour
Air-Circulation Dryer
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC-A2-1 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC-A1-10 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC-A1-2 Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Chute Hot-Wind
Zhejiang Juner PC-A1-9A Top-Grade Flame Retardant UV-Resistant
Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd.
Drying Temperature 120 °C

@Time 18000 sec
248 °F

@Time 5.00 hour
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..