| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..
|
|||
| Drying Temperature |
>=
150
°C @Time 10800 sec |
>=
302
°F @Time 3.00 hour |
|
|
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8102 PEEK, with PTFE, lubricant modified, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8432 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8496 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann..
|
|||
| Drying Temperature |
150
°C @Time >=14400 sec |
302
°F @Time >=4.00 hour |
or |
|
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Drying Temperature |
150
°C @Time >=14400 sec |
302
°F @Time >=4.00 hour |
or |
|
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Drying Temperature |
150
°C @Time >=14400 sec |
302
°F @Time >=4.00 hour |
or |
|
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Drying Temperature |
150
°C @Time 14400 - 21600 sec |
302
°F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
|
|||
| Drying Temperature |
150
°C @Time 14400 - 28800 sec |
302
°F @Time 4.00 - 8.00 hour |
Air-Circulation Dryer |
|
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/MS/15/TF/15 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/RD7405 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-0856/GY7 PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7583 PEEK, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Chemical and hydroly..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time >=14400 sec |
302
°F @Time >=4.00 hour |
or |
|
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8135/OR PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||