| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
|
|||
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
|
|||
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8173 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8174 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
|
|||
| Drying Temperature |
150
°C @Time >=14400 sec |
302
°F @Time >=4.00 hour |
or |
|
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Drying Temperature |
150
°C @Time 14400 - 28800 sec |
302
°F @Time 4.00 - 8.00 hour |
Air-Circulation Dryer |
|
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/BK PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-0895/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7018/GN PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/TF/20/BN PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 21600 sec |
302
°F @Time 3.00 - 6.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..
|
|||