| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7532 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 36000 - 57600 sec
|
167
°F <br>@Time 10.0 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 36000 sec
|
167
°F <br>@Time 6.00 - 10.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-7884 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 36000 sec
|
167
°F <br>@Time 6.00 - 10.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/CF/10/GK/20/TF/5/BK Polyamide 66, with carbon fiber, glass spheres and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/CF/20/HS Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/XCF/40 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-0889-5 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-1108 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-7943 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 7200 - 28800 sec
|
167
°F <br>@Time 2.00 - 8.00 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 80-8030 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® GS-H/2 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/BK Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/BK Polyamide 66, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1-8130 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
|
|||
| Drying Temperature |
75.0
°C <br>@Time 21600 - 57600 sec
|
167
°F <br>@Time 6.00 - 16.0 hour
|
Dehumidifying dryer |
|
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann ..
|
|||