| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
|
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d
Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not..
|
|||
| Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
|
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p..
|
|||
| Feed Temperature | 60.0 - 70.0 °C | 140 - 158 °F | Injection molding |
|
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..
|
|||
| Feed Temperature | 60.0 °C | 140 °F | |
|
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NB40 GR50 NL IL PA6, 50% glass fiber reinforced, impact modified, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NT40 GR15 NL HS PPA, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | <= 60.0 °C | <= 140 °F | Throat |
|
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Feed Temperature | <= 60.0 °C | <= 140 °F | Throat |
|
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Information provided by Eurotec®
|
|||