| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISBLEND® PC/ABS
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 15% Glass Fiber Reinforced and Heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 30% Glass Fiber Filled Reinforced Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Feed Temperature | 70.0 °C | 158 °F | |
|
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||