| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||
| Feed Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced
GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi..
|
|||
| Feed Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecotek® PC40 NL FA70 PC, unfilled, flame retardant - (RoHS compliant), natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey
Information provided by Eurotec®
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
|
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Feed Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
|
Borealis ME268Al Polypropylene Compound, Mineral Filled
ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par..
|
|||