| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR ..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well ..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
|
|||
| Adapter Temperature | 260 - 266 °C | 500 - 511 °F | Cast Film |
|
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a..
|
|||
| Adapter Temperature | 246 - 266 °C | 475 - 510 °F | |
|
Entec Hylex® P1302B Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||