| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Die Temperature | 225 - 295 °C | 437 - 563 °F | Average value: 265 °C Grade Count:3 |
|
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM
Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Conditioned (2.5% Moisture)
Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM
Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..
|
|||
| Die Temperature | 270 - 295 °C | 518 - 563 °F | |
|
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM
Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, ..
|
|||