Polymer Property : Zone 1 = 275 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded
Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 30Y D61 PA66, Carbon Fiber Filled, Injection Molded
Star L PA66 30Y D51 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 D51 PA66, Injection Molded
Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded
Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Staramide R1000K PA66, Injection Molded
Staramide R1000K is an Unreinforced Radiation Crosslinkable Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 255 - 275 °C
491 - 527 °F
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded
RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded
RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Staramide RX06027 PA66, 30% Glass Filled, Injection Molded
Staramide RX06027 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S34/8)Information provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 1 255 - 275 °C
491 - 527 °F
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded
Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar.
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Staramide RFM3353EM PA66/6, Glass/Mineral Fiber Reinforced, Injection Molding
Starflam RFM3353EM is a Mineral Filled, Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry)
Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the..
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® TG3S 15% Glass Filled PA6 (Conditioned)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned)
Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the..
Zone 1 230 - 275 °C
446 - 527 °F
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
Zone 1 245 - 275 °C
473 - 527 °F
Rear Zone
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Zone 1 265 - 275 °C
509 - 527 °F
Eurostar Star L PA66 15Y D61 PA66, Carbon Filled, Injection Molded
Star L PA66 15Y D61 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.