| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7488 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-RG 2 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/CF/10/GK/20/TF/5/BK Polyamide 66, with carbon fiber, glass spheres and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/CF/15/TF/20/BK Polyamide 66, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0936 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7701 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7893/GY Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7984 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/BK Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 1 | 290 - 310 °C | 554 - 590 °F | |
|
Lehmann & Voss LUVOCOM® 1-8227 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||