| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber
Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE
Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 1 | 330 - 350 °C | 626 - 662 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||