| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 260 - 280 °C | 500 - 536 °F | hopper |
|
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Zone 1 | 260 - 290 °C | 500 - 554 °F | hopper |
|
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
|
|||
| Zone 1 | 260 °C | 500 °F | |
|
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **)
Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw..
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Staramide A40 PA66, Extrusion
Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide ACF2 PA66, 10% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF2 is a 10% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Staramide R1000 PA66, Injection Molded
Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Staramide R1000IX4 PA66, Impact Modified, Injection Molded
Staramide R1000IX4 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI020 Star X 1020)Information provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide RF005S PA66, 25% Glass Fiber, Injection Molded
Starflam RF005S is a 25% Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding
Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding
Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Starflam RF0023K PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0023K is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding, Crosslinkable under Beta or Gamma RadiationInformation provided by Euros..
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding
Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 280 °C | 500 - 536 °F | |
|
Eurostar Staramide RF007ESS PA66/6, 35% Glass Filled, Injection Molded
Staramide RF007ESS is a 35% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as RF1007EMHS)Information provided by Eurostar.
|
|||
| Zone 1 | 260 - 270 °C | 500 - 518 °F | |
|
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 1 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 1 | 260 °C | 500 °F | Feeding zone |
|
BASF Ultradur® B 4520 High Speed PBT
Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF
|
|||
| Zone 1 | 260 °C | 500 °F | Feeding zone |
|
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
|
|||
| Zone 1 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 1 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 1 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 1 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 1 | 260 °C | 500 °F | Feed Zone |
|
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
|
|||
| Zone 1 | 260 °C | 500 °F | Feed Zone |
|
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
|
|||
| Zone 1 | 260 °C | 500 °F | Feed zone |
|
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..
|
|||
| Zone 1 | 260 °C | 500 °F | Feed Zone |
|
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
|
|||
| Zone 1 | 260 °C | 500 °F | Feed Zone |
|
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
|
|||
| Zone 1 | 260 °C | 500 °F | Feed Zone |
|
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
|
|||