| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
|
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 1700-8019 PPO, with glass fiber and PTFE, low-warpage
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Zone 1 | 270 - 290 °C | 518 - 554 °F | |
|
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar.
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar.
|
|||
| Zone 1 | 270 °C | 518 °F | Feed Zone |
|
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
|
|||
| Zone 1 | 270 °C | 518 °F | Feed Zone |
|
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
|
|||
| Zone 1 | 270 °C | 518 °F | Feed Zone |
|
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin..
|
|||
| Zone 1 | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
|
|||