| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 2 | 250 °C | 482 °F | Die |
|
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding
Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding
Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded
Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PX06009 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX06009 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded
Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PZ00062E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX0062E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded
Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded
Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam EXCP0132 PA, Mineral Filled, Injection Molding
Starflam EXCP0132 is a Halogen Free and Red Phosphorous Free, Mineral Filled, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 2 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM
Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h..
|
|||
| Zone 2 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Zone 2 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
|
|||
| Zone 2 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM
Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug..
|
|||
| Zone 2 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..
|
|||