Polymer Property : Zone 2 = 290 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66
Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Zone 2 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Zone 2 265 - 290 °C
509 - 554 °F
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Zone 2 270 - 290 °C
518 - 554 °F
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
Zone 2 250 - 290 °C
482 - 554 °F
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Zone 2 270 - 290 °C
518 - 554 °F
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded
Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.
Zone 2 270 - 290 °C
518 - 554 °F
Eurostar Staramide RFB53U PA66, 50% Glass Bead/Fiber Filled, Injection Molded
RFB53U is a Glass Bead/ Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 1525 VK Z4)Information provided by Eurostar.
Zone 2 270 - 290 °C
518 - 554 °F
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded
RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar.