Polymer Property : Zone 2 = 310 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Zone 2 310 - 340 °C
590 - 644 °F
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Zone 2 310 - 340 °C
590 - 644 °F
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec..
Zone 2 310 - 340 °C
590 - 644 °F
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Zone 2 310 - 340 °C
590 - 644 °F
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Zone 2 310 - 330 °C
590 - 626 °F
Eurostar Starglas GX061104 PSU
Starglas GX061104 is a PSU resin (also known as Starglas PSU A ¾)Information provided by Eurostar.
Zone 2 310 °C
590 °F
Compression
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Zone 2 310 °C
590 °F
Compression
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic..
Zone 2 310 - 330 °C
590 - 626 °F
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..