| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 320 - 330 °C | 608 - 626 °F | |
|
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8305 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
|
|||