| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7753/BL PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7907 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8173 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8355 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 2 | 340 - 390 °C | 644 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis..
|
|||
| Zone 2 | 340 - 390 °C | 644 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7107 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8127-1 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 2 | 340 - 390 °C | 644 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
|
|||
| Zone 2 | 380 - 390 °C | 716 - 734 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7107/BK PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||