Polymer Property : Zone 2 = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 220 - 260 °C
428 - 500 °F
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Zone 2 220 °C
428 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 2 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound
PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,..
Zone 2 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound
PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties..
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG..
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced
Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &..
Zone 2 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical KEYFLEX BT HB9242D Ester Type TPE
Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
Zone 2 220 °C
428 °F
Injection Molding
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Zone 2 220 °C
428 °F
Injection Molding
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U..
Zone 2 220 °C
428 °F
Injection Molding
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE.
Zone 2 220 °C
428 °F
Injection Molding
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat..
Zone 2 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 2 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 2 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 2 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 2 220 - 250 °C
428 - 482 °F
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..