Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 446 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 200 - 230 °C
392 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 2 210 - 230 °C
410 - 446 °F
Extrusion
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 2 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical MU620 ABS, Low Deformation
Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical PI641 ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS650 ABS
Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 200 - 230 °C
392 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
Zone 2 200 - 230 °C
392 - 446 °F
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Zone 2 200 - 230 °C
392 - 446 °F
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Zone 2 190 - 230 °C
374 - 446 °F
Eurostar Starflam MX06089 PP, Flame Retardant, Injection Molding
Starflam MX06089 is an Unfilled Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar.
Zone 2 220 - 230 °C
428 - 446 °F
Eurostar Starpylen M1000-BK1A987 PP, Carbon Black
Starpylen M1000-BK1A987 is a high carbon black load PP resinInformation provided by Eurostar.