Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 464 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 240 - 270 °C
464 - 518 °F
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
Zone 2 240 - 270 °C
464 - 518 °F
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
Zone 2 240 - 265 °C
464 - 509 °F
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price..
Zone 2 240 - 270 °C
464 - 518 °F
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
Zone 2 240 - 270 °C
464 - 518 °F
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-7433 Polyamide 12, with carbon fiber, hydrolysis resistant
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-7833 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-8503/BL Polyamide 12, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Zone 2 240 - 260 °C
464 - 500 °F
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic..
Zone 2 240 - 270 °C
464 - 518 °F
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide B40 PA6, Extrusion
Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded
Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide PF005 PA6, 25% Glass Fiber Filled, Injection Molded
Staramide PF005 is an 25% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide PF003U PA6, 15% Glass Fiber Filled, Injection Molded
Staramide PF003U is an 15% Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin, UV Stabilized (also known as Staramide 6 15V S4)Information provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded
Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 - 250 °C
464 - 482 °F
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Zone 2 240 °C
464 °F
Compression
BASF Ultramid® Seal-Fit PA6/66 (Conditioned)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved