Polymer Property : Zone 2 = 563 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM
Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM
Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..
Zone 2 250 - 295 °C
482 - 563 °F
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM
Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, ..