| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Zone 2 | 290 - 330 °C | 554 - 626 °F | |
|
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
|
|||
| Zone 2 | 320 - 330 °C | 608 - 626 °F | |
|
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||
| Zone 2 | 310 - 330 °C | 590 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||