| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst CAT 10 Polyolefin
Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin
Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst LV/1 Polyolefin
Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst LV/1LR Polyolefin
Catalyst LV/1LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or ..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin
Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/2 Polyolefin
Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam ..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin
Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin
Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or ..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin
Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Catalyst PS/4 Polyolefin
Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes...
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE)
POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
|
|||
| Zone 3 | 150 - 200 °C | 302 - 392 °F | |
|
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
|
|||
| Zone 3 | 150 - 170 °C | 302 - 338 °F | |
|
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE)
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S..
|
|||
| Zone 3 | 150 °C | 302 °F | |
|
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t..
|
|||
| Zone 3 | 150 °C | 302 °F | |
|
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable
Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP..
|
|||