| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 250 °C | 482 °F | |
|
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Zone 3 | 250 - 280 °C | 482 - 536 °F | |
|
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
|
|||
| Zone 3 | 250 - 280 °C | 482 - 536 °F | |
|
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding
Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide B28 PA6, Injection Molded
Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide B40 PA6, Extrusion
Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded
Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam EXCP0132 PA, Mineral Filled, Injection Molding
Starflam EXCP0132 is a Halogen Free and Red Phosphorous Free, Mineral Filled, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded
Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar.
|
|||
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
|
Eurostar Starflam PK00032E PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Starflam PK0032E is a Halogen Free Red Phosphorous Free Flame Retardant Mineral Filled Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM
Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h..
|
|||
| Zone 3 | 250 - 295 °C | 482 - 563 °F | |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||