| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber
Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified
Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by..
|
|||
| Zone 3 | 230 - 260 °C | 446 - 500 °F | |
|
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced
Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &..
|
|||
| Zone 3 | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Star L PA D51 PA6, Injection Molded
Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide B28N PA6, Nucleated, Injection Molded
Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide B40 PA6, Extrusion
Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded
Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Star L PA6 D61 PA6, Injection Molded
Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded
Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 250 - 260 °C | 482 - 500 °F | |
|
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Star L PA6 D83 PA6, Injection Molded
Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||