| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 245 - 285 °C | 473 - 545 °F | |
|
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
|
|||
| Zone 3 | 245 - 285 °C | 473 - 545 °F | |
|
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character..
|
|||
| Zone 3 | 245 - 285 °C | 473 - 545 °F | |
|
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
|
|||
| Zone 3 | 245 - 285 °C | 473 - 545 °F | |
|
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
|
|||
| Zone 3 | 245 - 285 °C | 473 - 545 °F | |
|
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
|
|||
| Zone 3 | 275 - 285 °C | 527 - 545 °F | |
|
Lehmann & Voss LUVOCOM® 8-7190 High impact polyamide, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR560B1 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR560B1 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR460B PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR460B is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Zone 3 | 270 - 285 °C | 518 - 545 °F | |
|
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||