Polymer Property : Zone 3 = 305 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-8019 PPO, with glass fiber and PTFE, low-warpage
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour...
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor..
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Zone 3 275 - 305 °C
527 - 581 °F
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Zone 3 275 - 305 °C
527 - 581 °F
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Zone 3 275 - 305 °C
527 - 581 °F
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..