| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry)
Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan..
|
|||
| Zone 3 | 320 °C | 608 °F | Metering-zone |
|
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | |
|
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
|
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses ..
|
|||
| Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
|
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses ..
|
|||
| Zone 3 | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||