| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 170 °C | 338 °F | |
|
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||
| Zone 3 | 170 - 200 °C | 338 - 392 °F | |
|
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **)
PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
|
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
|
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
|
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 180 °C | 338 - 356 °F | Injection Molding |
|
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
|
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 180 °C | 338 - 356 °F | Injection Molding |
|
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
|
|||
| Zone 3 | 170 - 180 °C | 338 - 356 °F | |
|
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
|
|||
| Zone 3 | 170 - 180 °C | 338 - 356 °F | |
|
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera..
|
|||
| Zone 3 | 170 - 179 °C | 338 - 355 °F | |
|
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
|
|||
| Zone 3 | 170 - 190 °C | 338 - 374 °F | |
|
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki..
|
|||
| Zone 3 | 170 °C | 338 °F | Extrusion |
|
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables..
|
|||
| Zone 3 | 170 °C | 338 °F | |
|
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable
Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m..
|
|||
| Zone 3 | 170 °C | 338 °F | |
|
Borealis Visico™/Visico™ LE4421/LE4438 Polyethylene Compound, Crosslinkable
Visico™ LE4421 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4421 and Visico™ LE4438 is a combination of a Visico™ bas..
|
|||
| Zone 3 | 170 °C | 338 °F | |
|
Borealis Visico™/Visico™ LE4423/LE4438 Polyethylene Compound, Crosslinkable
Visico™ LE4423 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ LE4423 and Visico™ LE4438 is a combination of a Visico™ bas..
|
|||
| Zone 3 | 170 °C | 338 °F | |
|
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable
Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442..
|
|||
| Zone 3 | 170 °C | 338 °F | Extrusion |
|
Lubrizol Estane® 54611 Polyester-Based Thermoplastic Polyurethane
Feature: Facilitates to produce high coating weight in one pass high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foils.Av..
|
|||
| Zone 3 | 170 °C | 338 °F | Blown Film Coextrusion |
|
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
|
|||