Polymer Property : Zone 3 = 350 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE
Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8217 Polyether imide, with PTFE, lubricant modified
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Control disks, cams, slidi..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 °C
662 °F
Metering-zone
BASF Ultrason® S 3010 MR UN PSU
Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7742 Polyether imide, with glass fiber, demolding aid
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..
Zone 3 350 - 400 °C
662 - 752 °F
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable
Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le..