| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
|
|||
| Zone 3 | 390 - 420 °C | 734 - 788 °F | |
|
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7994 PEEK, unreinforced
Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S..
|
|||
| Zone 3 | 390 - 420 °C | 734 - 788 °F | |
|
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Zone 3 | 390 - 420 °C | 734 - 788 °F | |
|
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/CF/15/TF/15 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8339 PEEK, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||