Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 3 = 428 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 3 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Zone 3 220 °C
428 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Zone 3 220 °C
428 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Zone 3 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 3 220 °C
428 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1391 Conductive Thermoplastic Compound
PRE-ELEC® PP 1391 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 3 220 °C
428 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 3 220 - 300 °C
428 - 572 °F
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Zone 3 220 - 240 °C
428 - 464 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 3 220 °C
428 °F
Injection Molding
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JI6L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: for multilayer tubeInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Hexane for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030XA Nylon 12 Film
Description: UBESTA Nylon 12 FilmInformation provided by UBE.
Zone 3 220 - 230 °C
428 - 446 °F
Eurostar Starglas FX05032 PE
Starglas FX05032 is Polyethylene Resin with a Proprietary Additive (foaming agent for polyolefins)Information provided by Eurostar.
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 3 220 °C
428 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Copyright © lookpolymers.com All Rights Reserved